Figure 6

LEED patterns, (a) after the third NH3 flux anneal, the electron kinetic energy was 104 eV, (b) after the last surface cleaning consisting of Ga deposition during heating followed by NH3 flux anneal, the electron kinetic energy was 147 eV.


(click for full image)

top        text     Figure 5     Figure 7        endnotes

last updated Tuesday, October 18, 2005 1:34:01 PM.

© 2004-2005 The Materials Research Society MRS Internet Journal of Nitride Semiconductor Research