Figure 43

Reverse leakage current measured at -30 V for GaN p-i-n junctions etched in ICP 32Cl2/8BCl3/5Ar discharges (-300 V dc chuck self-bias, 500 W ICP source power, 2 mTorr), as a function of anneal temperature.