Figure 3

Indium content in InGaN grown in AIX-200 horizontal reactor as a function of substrate temperature at high In/(In+Ga) gas phase ratio. The reactor pressure is 50 mbar. Solid line presents the modeling results, circles are the experimental data.


top        text     Figure 2     Figure 4        endnotes